Issue link: http://read.dmtmag.com/i/814629
Technical Training and Reference Info Lubrication Technical Training 1 800 255 4417 www.castrol.com/GPS March 2017 Gears Methods of Lubricant Application Running-In Open Gears Running-in open gear drives is a metal-removal process designed to increase the contact area between the gears. It is imperative that drives be properly aligned and at operating temperature before attempting a running-in or dressing process. Improper procedures can result in devastating damage to the gears (Figure 12). Figure 12. Example of harsh abrasive applied to the distressed areas of the loaded pressure flanks of a pinion. Consult With a Technical Expert before Attempting Run-In or Dressing of Open Gears! Consideration should be given to the following before attempting running-in or dressing the gears: • Moderate wear or damage may be removed through the use of a suitable run-in compound (such as Castrol Molub-Alloy OG-RI) • Heavy wear or damage, if not too severe, requires a two-step process, consisting of heavy run-in with a harsh abrasive followed by normal run-in compound • Severe damage may require gear reversal or replacement • Heavy dressing with a special abrasive can take from 3 to 24 hours, depending on gear and pinion flank condition. • Light dressing with run-in compound can take from 72 to 240 hours to polish the pressure flanks fully • New or light-to-moderately worn bull gears mated to new pinion flanks may only require use of a run-in compound • New pinion mated to new bull gear flanks can take from 5 to 14 days to fully run-in using a run-in compound • New pinion flanks mated to worn bull gear flanks may require a two-step process that can take from 5 to 21 days Gear Failure and Troubleshooting The most common gear wear occurs when pits and/or fatigue cracks initiate either at the surface of the gear tooth or at depth below the surface. The cracks tend to propagate toward each other, as shown in Figure 13. Figure 13. Propagation of cracks below the metal surface. Credit: Bruce T. Kuhnell "Wear in Rolling Element Bearings and Gears," Machinery Lubrication Magazine, 2007. Pitting is the formation of shallow craters by surface- defect fatigue, and spalling is the formation of deeper cavities due to subsurface-defect fatigue. Figure 14 shows a large single spall over 250 µm across. Initial spall particles are typically 30 µm to 50 µm, but it is common for several particles to be generated from individual spall sites. Note that at the sharper crater wall (near the top edge of the spall in this micrograph), there are several cracks associated with the spall. Figure 14. Large spall, 250 µm across. Credit: Bruce T. Kuhnell "Wear in Rolling Element Bearings and Gears," Machinery Lubrication Magazine, 2007. R33